Mechanical

Hardness, Rockwell F HRF

88 - 95 [-] at 20 °C

Hardness, Rockwell Superficial 30-T HRB 30-T

56 - 64 [-] at 20 °C

Tensile strength Rm

325 - 385 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

99.4 %

As

0.15 - 0.5 %

P

0.02 - 0.04 %