ASTM B171 Grade C46400 M20, M10, O20, and O25

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by ASTM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A50

20.0 °C

35 %

Show Material materials with Elongation A50 of 35 %

Tensile strength

20.0 °C

345 MPa

Show Material materials with Tensile strength of 345 MPa

Yield Strength Rp0.2, short transverse

20.0 °C

125 - 140 MPa

Show Material materials with Yield Strength Rp0.2, short transverse of 125 - 140 MPa

Yield strength Rp0.5

20.0 °C

125 - 140 MPa

Show Material materials with Yield strength Rp0.5 of 125 - 140 MPa

Chemical properties

PropertyValue

Copper

59 - 62 %

Show Material materials with Copper of 59 - 62 %

Iron

0.1 %

Show Material materials with Iron of 0.1 %

Lead

0.2 %

Show Material materials with Lead of 0.2 %

Tin

0.5 - 1 %