Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 10 % Show Material materials with Elongation A50 of 10 % |
Tensile strength | 20.0 °C | 550 - 620 MPa Show Material materials with Tensile strength of 550 - 620 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 195 - 235 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 195 - 235 MPa |
Yield strength Rp0.5 | 20.0 °C | 205 - 250 MPa Show Material materials with Yield strength Rp0.5 of 205 - 250 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 9 - 11 % Show Material materials with Aluminium of 9 - 11 % |
Iron | 2 - 4 % Show Material materials with Iron of 2 - 4 % |
Manganese | 1.5 % Show Material materials with Manganese of 1.5 % |
Nickel | 4 - 5.5 % Show Material materials with Nickel of 4 - 5.5 % |
Tin | 0.2 % Show Material materials with Tin of 0.2 % |
Zinc | 0.3 % Show Material materials with Zinc of 0.3 % |