Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 10 % Show Material materials with Elongation A50 of 10 % |
Tensile strength | 20.0 °C | 550 - 620 MPa Show Material materials with Tensile strength of 550 - 620 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 195 - 235 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 195 - 235 MPa |
Yield strength Rp0.5 | 20.0 °C | 205 - 250 MPa Show Material materials with Yield strength Rp0.5 of 205 - 250 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 8.7 - 9.5 % Show Material materials with Aluminium of 8.7 - 9.5 % |
Iron | 3.5 - 4.3 % Show Material materials with Iron of 3.5 - 4.3 % |
Lead | 0.02 % Show Material materials with Lead of 0.02 % |
Manganese | 1.2 - 2 % Show Material materials with Manganese of 1.2 - 2 % |
Nickel | 4 - 4.8 % Show Material materials with Nickel of 4 - 4.8 % |