Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 30 % Show Material materials with Elongation A50 of 30 % |
Tensile strength | 20.0 °C | 275 MPa Show Material materials with Tensile strength of 275 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 105 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 105 MPa |
Yield strength Rp0.5 | 20.0 °C | 105 MPa Show Material materials with Yield strength Rp0.5 of 105 MPa |
Chemical properties
Property | Value |
---|---|
Copper | 86.5 % Show Material materials with Copper of 86.5 % |
Iron | 1 - 1.8 % Show Material materials with Iron of 1 - 1.8 % |
Lead | 0.02 % Show Material materials with Lead of 0.02 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Nickel | 9 - 11 % Show Material materials with Nickel of 9 - 11 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |