Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 30 % Show Material materials with Elongation A50 of 30 % |
Tensile strength | 20.0 °C | 310 - 345 MPa Show Material materials with Tensile strength of 310 - 345 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 125 - 140 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 125 - 140 MPa |
Yield strength Rp0.5 | 20.0 °C | 125 - 140 MPa Show Material materials with Yield strength Rp0.5 of 125 - 140 MPa |
Chemical properties
Property | Value |
---|---|
Copper | 65 % Show Material materials with Copper of 65 % |
Iron | 0.4 - 1 % Show Material materials with Iron of 0.4 - 1 % |
Lead | 0.02 % Show Material materials with Lead of 0.02 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Nickel | 29 - 33 % Show Material materials with Nickel of 29 - 33 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |