Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 35 % Show Material materials with Elongation A50 of 35 % |
Tensile strength | 20.0 °C | 290 MPa Show Material materials with Tensile strength of 290 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 110 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 110 MPa |
Yield strength Rp0.5 | 20.0 °C | 110 MPa Show Material materials with Yield strength Rp0.5 of 110 MPa |
Chemical properties
Property | Value |
---|---|
Chromium | 0.3 - 0.7 % Show Material materials with Chromium of 0.3 - 0.7 % |
Iron | 0.5 - 1 % Show Material materials with Iron of 0.5 - 1 % |
Lead | 0.05 % Show Material materials with Lead of 0.05 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Nickel | 15 - 18 % Show Material materials with Nickel of 15 - 18 % |
Zinc | 1 % Show Material materials with Zinc of 1 % |