ASTM B187 Grade C10500 O60

.XLSX
.PDF
Save

Description

Related Standards

Properties

Mechanical

Elongation A50 A50

25 % at 20 °C

Hardness, Rockwell C HRC

50 [-] at 20 °C

Tensile strength Rm

195 - 255 MPa at 20 °C

Yield strength YS

55 MPa at 20 °C

Electrical

Electrical resistivity ρel

1.72E-8 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

99.95 %

O

1E-3 %

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.