Mechanical

Elongation A50 A50

12 % at 20 °C

Hardness, Rockwell C HRC

23 [-] at 20 °C

Hardness, Rockwell Superficial 15-N HR 15-N

72 [-] at 20 °C

Hardness, Rockwell Superficial 30-N HR 30-N

44 [-] at 20 °C

Tensile strength Rm

825 - 930 MPa at 20 °C

Yield strength YS

655 - 860 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Be

1.8 - 2 %

Al

0.2 %

Co

0.2 %

Si

0.2 %