ASTM B194 Grade C17200 TM05

.XLSX
.PDF
Save

Description

Related Standards

Properties

Mechanical

Elongation A50 A50

9 % at 20 °C

Hardness, Rockwell C HRC

31 [-] at 20 °C

Hardness, Rockwell Superficial 15-N HR 15-N

75.5 [-] at 20 °C

Hardness, Rockwell Superficial 30-N HR 30-N

52 [-] at 20 °C

Tensile strength Rm

1035 - 1105 MPa at 20 °C

Yield strength YS

860 - 965 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Be

1.8 - 2 %

Al

0.2 %

Co

0.2 %

Si

0.2 %

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.