ASTM B196 Grade C17300 TF00

.XLSX
.PDF
Save

Description

Related Standards

Properties

Mechanical

Elongation A50 A50

3 - 4 % at 20 °C

Hardness, Rockwell B HRB

36 - 42 [-] at 20 °C

Tensile strength Rm

1140 - 1380 MPa at 20 °C

Yield Strength Rp0.2, short transverse Rp0.2,shorttrans_

900 - 1000 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Be

1.8 - 2 %

Al

0.2 %

Pb

0.2 - 0.6 %

Si

0.2 %

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.