ASTM B196 Grade C17300 TH04

Want to keep this datasheet? Save it now in your required format

Description

Related Standards

Equivalent Materials

Properties

Mechanical

Elongation A50

A50

2 - 4 % at 20 °C

Hardness, Rockwell B

HRB

37 - 45 [-] at 20 °C

Tensile strength

Rm

1210 - 1550 MPa at 20 °C

Yield strength Rp0.2

Rp0.2

1000 - 1100 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

1.6E-5 - 1.8E-5 1/K at 20 °C

Typical for Wrought Copper High Copper Alloy

Specific heat capacity

cp

360 - 420 J/(kg·K) at 20 °C

Typical for Wrought Copper High Copper Alloy

Chemical properties

Element

Weight %

Comment

Be

1.8 - 2 %

Al

0.2 %

Pb

0.2 - 0.6 %

Si

0.2 %

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.