Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 96 - 120 GPa Show Material materials with Elastic modulus of 96 - 120 GPa | Typical for Cast Copper Bronze |
Elongation A50 | 23.0 °C | 15 % Show Material materials with Elongation A50 of 15 % | |
Poisson's ratio | 23.0 °C | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Bronze |
Tensile strength | 23.0 °C | 207 MPa Show Material materials with Tensile strength of 207 MPa | |
Yield strength Rp0.5 | 23.0 °C | 97 MPa Show Material materials with Yield strength Rp0.5 of 97 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.9E-5 1/K | Typical for Cast Copper Bronze |
Melting point | 760 - 1060 °C Show Material materials with Melting point of 760 - 1060 °C | Typical for Cast Copper Bronze | |
Specific heat capacity | 23.0 °C | 376 - 440 J/(kg·K) Show Material materials with Specific heat capacity of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Thermal conductivity | 23.0 °C | 12 - 81 W/(m·K) Show Material materials with Thermal conductivity of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Chemical properties
Property | Value |
---|---|
Aluminium | 5E-3 % Show Material materials with Aluminium of 5E-3 % |
Antimony | 0.35 % Show Material materials with Antimony of 0.35 % |
Copper | 81 - 85 % Show Material materials with Copper of 81 - 85 % |
Iron | 0.2 % Show Material materials with Iron of 0.2 % |
Lead | 6 - 8 % Show Material materials with Lead of 6 - 8 % |
Nickel | 1 % Show Material materials with Nickel of 1 % |
Phosphorus | 0.15 % Show Material materials with Phosphorus of 0.15 % |
Silicon | 5E-3 % Show Material materials with Silicon of 5E-3 % |
Sulfur | 0.08 % Show Material materials with Sulfur of 0.08 % |
Tin | 6.3 - 7.5 % Show Material materials with Tin of 6.3 - 7.5 % |
Zinc | 1 - 4 % Show Material materials with Zinc of 1 - 4 % |