Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 40 % Show Material materials with Elongation A50 of 40 % |
Hardness, Rockwell F | 20.0 °C | 37 [-] Show Material materials with Hardness, Rockwell F of 37 [-] |
Tensile strength | 20.0 °C | 230 MPa Show Material materials with Tensile strength of 230 MPa |
Yield strength Rp0.5 | 20.0 °C | 75 MPa Show Material materials with Yield strength Rp0.5 of 75 MPa |
Chemical properties
Property | Value |
---|---|
Copper | 99.9 % Show Material materials with Copper of 99.9 % |