Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 35 % Show Material materials with Elongation A50 of 35 % |
Hardness, Rockwell F | 20.0 °C | 40 [-] Show Material materials with Hardness, Rockwell F of 40 [-] |
Tensile strength | 20.0 °C | 235 MPa Show Material materials with Tensile strength of 235 MPa |
Yield strength Rp0.5 | 20.0 °C | 85 MPa Show Material materials with Yield strength Rp0.5 of 85 MPa |
Chemical properties
Property | Value |
---|---|
Copper | 99.9 % Show Material materials with Copper of 99.9 % |
Phosphorus | 0 - 0.01 % Show Material materials with Phosphorus of 0 - 0.01 % |
Tellurium | 0.4 - 0.7 % Show Material materials with Tellurium of 0.4 - 0.7 % |