Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 40 % Show Material materials with Elongation A50 of 40 % |
Hardness, Rockwell B | 20.0 °C | 45 [-] Show Material materials with Hardness, Rockwell B of 45 [-] |
Tensile strength | 20.0 °C | 400 MPa Show Material materials with Tensile strength of 400 MPa |
Yield strength Rp0.5 | 20.0 °C | 160 MPa Show Material materials with Yield strength Rp0.5 of 160 MPa |
Chemical properties
Property | Value |
---|---|
Copper | 58 - 61 % Show Material materials with Copper of 58 - 61 % |
Iron | 0.15 % Show Material materials with Iron of 0.15 % |
Lead | 0.25 - 0.7 % Show Material materials with Lead of 0.25 - 0.7 % |
Tin | 0.25 % Show Material materials with Tin of 0.25 % |