Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 32 % Show Material materials with Elongation A50 of 32 % |
Hardness, Rockwell B | 20.0 °C | 82 [-] Show Material materials with Hardness, Rockwell B of 82 [-] |
Tensile strength | 20.0 °C | 565 MPa Show Material materials with Tensile strength of 565 MPa |
Yield strength Rp0.5 | 20.0 °C | 255 MPa Show Material materials with Yield strength Rp0.5 of 255 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 8.5 - 10 % Show Material materials with Aluminium of 8.5 - 10 % |
Iron | 3 - 4.5 % Show Material materials with Iron of 3 - 4.5 % |
Lead | 0.02 % Show Material materials with Lead of 0.02 % |
Tin | 0.6 % Show Material materials with Tin of 0.6 % |
Zinc | 0.8 % Show Material materials with Zinc of 0.8 % |