Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 35 % Show Material materials with Elongation A50 of 35 % |
Hardness, Rockwell B | 20.0 °C | 77 [-] Show Material materials with Hardness, Rockwell B of 77 [-] |
Tensile strength | 20.0 °C | 570 MPa Show Material materials with Tensile strength of 570 MPa |
Yield strength Rp0.5 | 20.0 °C | 285 MPa Show Material materials with Yield strength Rp0.5 of 285 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 6.3 - 7 % Show Material materials with Aluminium of 6.3 - 7 % |
Arsenic | 0.09 % Show Material materials with Arsenic of 0.09 % |
Iron | 0.3 % Show Material materials with Iron of 0.3 % |
Lead | 0.05 % Show Material materials with Lead of 0.05 % |
Manganese | 0.1 % Show Material materials with Manganese of 0.1 % |
Nickel | 0.25 % Show Material materials with Nickel of 0.25 % |
Silicon | 1.5 - 2 % Show Material materials with Silicon of 1.5 - 2 % |
Tin | 0.2 % Show Material materials with Tin of 0.2 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |