Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 33 % Show Material materials with Elongation A50 of 33 % |
Hardness, Rockwell B | 20.0 °C | 69 [-] Show Material materials with Hardness, Rockwell B of 69 [-] |
Tensile strength | 20.0 °C | 495 MPa Show Material materials with Tensile strength of 495 MPa |
Yield strength Rp0.5 | 20.0 °C | 235 MPa Show Material materials with Yield strength Rp0.5 of 235 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.25 % Show Material materials with Aluminium of 0.25 % |
Copper | 57 - 60 % Show Material materials with Copper of 57 - 60 % |
Iron | 0.8 - 2 % Show Material materials with Iron of 0.8 - 2 % |
Lead | 0.2 % Show Material materials with Lead of 0.2 % |
Manganese | 0.05 - 0.5 % Show Material materials with Manganese of 0.05 - 0.5 % |
Tin | 0.5 - 1.5 % Show Material materials with Tin of 0.5 - 1.5 % |