Mechanical
Property | Temperature | Value |
---|---|---|
Elongation A50 | 20.0 °C | 25 % Show Material materials with Elongation A50 of 25 % |
Hardness, Rockwell B | 20.0 °C | 73 [-] Show Material materials with Hardness, Rockwell B of 73 [-] |
Tensile strength | 20.0 °C | 570 MPa Show Material materials with Tensile strength of 570 MPa |
Yield strength Rp0.5 | 20.0 °C | 250 MPa Show Material materials with Yield strength Rp0.5 of 250 MPa |