Mechanical
Chemical properties
Property | Value |
---|---|
Carbon | 0.1 % Show Material materials with Carbon of 0.1 % |
Iron | 1 - 1.8 % Show Material materials with Iron of 1 - 1.8 % |
Lead | 0.01 % Show Material materials with Lead of 0.01 % |
Manganese | 1.5 % Show Material materials with Manganese of 1.5 % |
Nickel | 9 - 11 % Show Material materials with Nickel of 9 - 11 % |
Niobium | 1 % Show Material materials with Niobium of 1 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.5 % Show Material materials with Silicon of 0.5 % |
Sulfur | 0.02 % Show Material materials with Sulfur of 0.02 % |