Mechanical
Chemical properties
Property | Value |
---|---|
Carbon | 0.15 % Show Material materials with Carbon of 0.15 % |
Iron | 0.25 - 1.5 % Show Material materials with Iron of 0.25 - 1.5 % |
Lead | 0.01 % Show Material materials with Lead of 0.01 % |
Manganese | 1.5 % Show Material materials with Manganese of 1.5 % |
Nickel | 28 - 32 % Show Material materials with Nickel of 28 - 32 % |
Niobium | 0.5 - 1.5 % Show Material materials with Niobium of 0.5 - 1.5 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.5 % Show Material materials with Silicon of 0.5 % |