Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 110 - 130 GPa Show Material materials with Elastic modulus of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Elongation A50 | 23.0 °C | 4 - 12 % Show Material materials with Elongation A50 of 4 - 12 % | |
Tensile strength | 23.0 °C | 540 MPa Show Material materials with Tensile strength of 540 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Melting point | 855 - 1090 °C Show Material materials with Melting point of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Specific heat capacity | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Specific heat capacity of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Iron | 0.1 % Show Material materials with Iron of 0.1 % |
Nickel | 0.8 - 1.2 % Show Material materials with Nickel of 0.8 - 1.2 % |
Phosphorus | 0.03 - 0.07 % Show Material materials with Phosphorus of 0.03 - 0.07 % |
Tin | 0.7 - 1.1 % Show Material materials with Tin of 0.7 - 1.1 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |