Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 110 - 130 GPa Show Material materials with Elastic modulus of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Hardness, Rockwell B | 23.0 °C | 68 - 74 [-] Show Material materials with Hardness, Rockwell B of 68 - 74 [-] | |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 66 - 71 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 66 - 71 [-] | |
Tensile strength | 23.0 °C | 415 - 485 MPa Show Material materials with Tensile strength of 415 - 485 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Melting point | 855 - 1090 °C Show Material materials with Melting point of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Specific heat capacity | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Specific heat capacity of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Copper | 98.5 % Show Material materials with Copper of 98.5 % |
Iron | 0.8 - 1.2 % Show Material materials with Iron of 0.8 - 1.2 % |
Lead | 0.03 % Show Material materials with Lead of 0.03 % |
Phosphorus | 0.01 - 0.04 % Show Material materials with Phosphorus of 0.01 - 0.04 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |