General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 8.95 g/cm³ Show Material materials with Density of 8.95 g/cm³ | Typical for Wrought Copper Nickel Grade |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 120 - 156 GPa Show Material materials with Elastic modulus of 120 - 156 GPa | Typical for Wrought Copper Nickel Grade |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 45 - 70 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 45 - 70 [-] | |
Tensile strength | 23.0 °C | 310 MPa Show Material materials with Tensile strength of 310 MPa | |
Yield strength Rp0.5 | 23.0 °C | 240 MPa Show Material materials with Yield strength Rp0.5 of 240 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.4E-5 - 1.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.4E-5 - 1.8E-5 1/K | Typical for Wrought Copper Nickel Grade |
Melting point | 915 - 1240 °C Show Material materials with Melting point of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade | |
Specific heat capacity | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Specific heat capacity of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Thermal conductivity | 23.0 °C | 21 - 195 W/(m·K) Show Material materials with Thermal conductivity of 21 - 195 W/(m·K) | Typical for Wrought Copper Nickel Grade |
Chemical properties