General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 8.95 g/cm³ Show Material materials with Density of 8.95 g/cm³ | Typical for Wrought Copper Nickel Grade |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 120 - 156 GPa Show Material materials with Elastic modulus of 120 - 156 GPa | Typical for Wrought Copper Nickel Grade |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 67 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 67 [-] | |
Tensile strength | 23.0 °C | 380 MPa Show Material materials with Tensile strength of 380 MPa | |
Yield strength Rp0.5 | 23.0 °C | 305 MPa Show Material materials with Yield strength Rp0.5 of 305 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.4E-5 - 1.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.4E-5 - 1.8E-5 1/K | Typical for Wrought Copper Nickel Grade |
Melting point | 915 - 1240 °C Show Material materials with Melting point of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade | |
Specific heat capacity | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Specific heat capacity of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Thermal conductivity | 23.0 °C | 21 - 195 W/(m·K) Show Material materials with Thermal conductivity of 21 - 195 W/(m·K) | Typical for Wrought Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Chromium | 0.3 - 0.7 % Show Material materials with Chromium of 0.3 - 0.7 % |
Iron | 0.5 - 1 % Show Material materials with Iron of 0.5 - 1 % |
Lead | 0.05 % Show Material materials with Lead of 0.05 % |
Manganese | 1 % Show Material materials with Manganese of 1 % |
Nickel | 15 - 18 % Show Material materials with Nickel of 15 - 18 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Sulfur | 0.02 % Show Material materials with Sulfur of 0.02 % |
Zinc | 1 % Show Material materials with Zinc of 1 % |