Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 96 - 120 GPa Show Material materials with Elastic modulus of 96 - 120 GPa | Typical for Cast Copper Bronze |
Elongation A50 | 23.0 °C | 8 % Show Material materials with Elongation A50 of 8 % | |
Poisson's ratio | 23.0 °C | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Bronze |
Tensile strength | 23.0 °C | 310 MPa Show Material materials with Tensile strength of 310 MPa | |
Yield strength Rp0.5 | 23.0 °C | 172 MPa Show Material materials with Yield strength Rp0.5 of 172 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.9E-5 1/K | Typical for Cast Copper Bronze |
Melting point | 760 - 1060 °C Show Material materials with Melting point of 760 - 1060 °C | Typical for Cast Copper Bronze | |
Specific heat capacity | 23.0 °C | 376 - 440 J/(kg·K) Show Material materials with Specific heat capacity of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Thermal conductivity | 23.0 °C | 12 - 81 W/(m·K) Show Material materials with Thermal conductivity of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Chemical properties
Property | Value |
---|---|
Aluminium | 5E-3 % Show Material materials with Aluminium of 5E-3 % |
Antimony | 0.25 % Show Material materials with Antimony of 0.25 % |
Copper | 82 - 86 % Show Material materials with Copper of 82 - 86 % |
Iron | 0.2 % Show Material materials with Iron of 0.2 % |
Lead | 2 - 3.2 % Show Material materials with Lead of 2 - 3.2 % |
Nickel | 2.8 - 4 % Show Material materials with Nickel of 2.8 - 4 % |
Phosphorus | 1.5 % Show Material materials with Phosphorus of 1.5 % |
Silicon | 5E-3 % Show Material materials with Silicon of 5E-3 % |
Sulfur | 0.05 % Show Material materials with Sulfur of 0.05 % |
Tin | 9 - 11 % Show Material materials with Tin of 9 - 11 % |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % |