General
Property | Value | Comment |
---|---|---|
Density | 7.69 g/cm³ Show Material materials with Density of 7.69 g/cm³ | Predicted Value |
Grain size | 0.0305 μm Show Material materials with Grain size of 0.0305 μm | Predicted Value |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Compressive strength | 1181 MPa Show Material materials with Compressive strength of 1181 MPa | Predicted Value | |||
Elastic modulus | 96 - 120 GPa Show Material materials with Elastic modulus of 96 - 120 GPa | Typical for Cast Copper Bronze | |||
Fatigue strength | 381 MPa Show Material materials with Fatigue strength of 381 MPa | Predicted Value | |||
Hardness, Brinell | 151 [-] Show Material materials with Hardness, Brinell of 151 [-] | Predicted Value | |||
Hardness, HBW | 235.4 [-] Show Material materials with Hardness, HBW of 235.4 [-] | Predicted Value | |||
Hardness, Rockwell F | 74 [-] Show Material materials with Hardness, Rockwell F of 74 [-] | Predicted Value | |||
Hardness, Rockwell Superficial 15-N | 71 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 71 [-] | Predicted Value | |||
Hardness, Rockwell Superficial 30-N | 43 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 43 [-] | Predicted Value | |||
Hardness, Rockwell Superficial 30-T | 65 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 65 [-] | Predicted Value | |||
Hardness, Vickers | 161 [-] Show Material materials with Hardness, Vickers of 161 [-] | Predicted Value | |||
Poisson's ratio | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Bronze | |||
Reduction of area | 46.4 % Show Material materials with Reduction of area of 46.4 % | Predicted Value | |||
Shear modulus | 45.8 GPa Show Material materials with Shear modulus of 45.8 GPa | Predicted Value | |||
Shear strength | 324.8 MPa Show Material materials with Shear strength of 324.8 MPa | Predicted Value | |||
Tensile strength | 483 MPa Show Material materials with Tensile strength of 483 MPa | Heat-Treated | ASTM B505 | Casting |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.6e-05 - 1.9e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Melting point | 760 - 1060 °C Show Material materials with Melting point of 760 - 1060 °C | Typical for Cast Copper Bronze |
Specific heat capacity | 376 - 440 J/(kg·K) Show Material materials with Specific heat capacity of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Thermal conductivity | 12 - 81 W/(m·K) Show Material materials with Thermal conductivity of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Electrical
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 9 - 11 % Show Material materials with Aluminium of 9 - 11 % | Heat-Treated | ASTM B505 | Casting |
Copper | 86 % Show Material materials with Copper of 86 % | Heat-Treated | ASTM B505 | Casting |
Iron | 0.8 - 1.5 % Show Material materials with Iron of 0.8 - 1.5 % | Heat-Treated | ASTM B505 | Casting |