General
Property | Value | Comment |
---|---|---|
Density | 7.692 g/cm³ Show Material materials with Density of 7.692 g/cm³ | Predicted Value |
Grain size | 0.031 μm Show Material materials with Grain size of 0.031 μm | Predicted Value |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Compressive strength | 1181 MPa Show Material materials with Compressive strength of 1181 MPa | Predicted Value | |||
Elastic modulus | 96 - 120 GPa Show Material materials with Elastic modulus of 96 - 120 GPa | Typical for Cast Copper Bronze | |||
Fatigue strength | 384 MPa Show Material materials with Fatigue strength of 384 MPa | Predicted Value | |||
Hardness, Brinell | 152 [-] Show Material materials with Hardness, Brinell of 152 [-] | Predicted Value | |||
Hardness, HBW | 235 [-] Show Material materials with Hardness, HBW of 235 [-] | Predicted Value | |||
Hardness, Rockwell F | 77 [-] Show Material materials with Hardness, Rockwell F of 77 [-] | Predicted Value | |||
Hardness, Rockwell Superficial 15-N | 71 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 71 [-] | Predicted Value | |||
Hardness, Rockwell Superficial 30-N | 44 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 44 [-] | Predicted Value | |||
Hardness, Rockwell Superficial 30-T | 68 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 68 [-] | Predicted Value | |||
Hardness, Vickers | 168 [-] Show Material materials with Hardness, Vickers of 168 [-] | Predicted Value | |||
Poisson's ratio | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Bronze | |||
Reduction of area | 43.7 % Show Material materials with Reduction of area of 43.7 % | Predicted Value | |||
Shear modulus | 45.0 GPa Show Material materials with Shear modulus of 45.0 GPa | Predicted Value | |||
Shear strength | 296.2 MPa Show Material materials with Shear strength of 296.2 MPa | Predicted Value | |||
Tensile strength | 552 MPa Show Material materials with Tensile strength of 552 MPa | HT, Heat-Treated | ASTM B505 | Casting |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.6e-05 - 1.9e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Melting point | 760 - 1060 °C Show Material materials with Melting point of 760 - 1060 °C | Typical for Cast Copper Bronze |
Specific heat capacity | 376 - 440 J/(kg·K) Show Material materials with Specific heat capacity of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Thermal conductivity | 12 - 81 W/(m·K) Show Material materials with Thermal conductivity of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Electrical
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 9 - 11 % Show Material materials with Aluminium of 9 - 11 % | HT, Heat-Treated | ASTM B505 | Casting |
Copper | 86 % Show Material materials with Copper of 86 % | HT, Heat-Treated | ASTM B505 | Casting |
Iron | 0.8 - 1.5 % Show Material materials with Iron of 0.8 - 1.5 % | HT, Heat-Treated | ASTM B505 | Casting |