General
Property | Value | Comment |
---|---|---|
Density | 7.592 g/cm³ Show Material materials with Density of 7.592 g/cm³ | Predicted Value |
Grain size | 0.0311 μm Show Material materials with Grain size of 0.0311 μm | Predicted Value |
Mechanical
Property | Value | Comment |
---|---|---|
Compressive strength | 1182 MPa Show Material materials with Compressive strength of 1182 MPa | Predicted Value |
Elastic modulus | 96 - 120 GPa Show Material materials with Elastic modulus of 96 - 120 GPa | Typical for Cast Copper Bronze |
Fatigue strength | 376 MPa Show Material materials with Fatigue strength of 376 MPa | Predicted Value |
Hardness, Brinell | 155 [-] Show Material materials with Hardness, Brinell of 155 [-] | Predicted Value |
Hardness, HBW | 251.3 [-] Show Material materials with Hardness, HBW of 251.3 [-] | Predicted Value |
Hardness, Rockwell F | 82 [-] Show Material materials with Hardness, Rockwell F of 82 [-] | Predicted Value |
Hardness, Rockwell Superficial 15-N | 74 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 74 [-] | Predicted Value |
Hardness, Rockwell Superficial 30-N | 47 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 47 [-] | Predicted Value |
Hardness, Rockwell Superficial 30-T | 89 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 89 [-] | Predicted Value |
Hardness, Vickers | 236 [-] Show Material materials with Hardness, Vickers of 236 [-] | Predicted Value |
Poisson's ratio | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Bronze |
Reduction of area | 35.7 % Show Material materials with Reduction of area of 35.7 % | Predicted Value |
Shear modulus | 46.4 GPa Show Material materials with Shear modulus of 46.4 GPa | Predicted Value |
Shear strength | 420.7 MPa Show Material materials with Shear strength of 420.7 MPa | Predicted Value |
Yield strength | 563.7 MPa Show Material materials with Yield strength of 563.7 MPa | Predicted Value, RP02 |
621.1 MPa Show Material materials with Yield strength of 621.1 MPa | Predicted Value | |
708.3 MPa Show Material materials with Yield strength of 708.3 MPa | Predicted Value, RP005 |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.6e-05 - 1.9e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Melting point | 760 - 1060 °C Show Material materials with Melting point of 760 - 1060 °C | Typical for Cast Copper Bronze |
Specific heat capacity | 376 - 440 J/(kg·K) Show Material materials with Specific heat capacity of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Thermal conductivity | 12 - 81 W/(m·K) Show Material materials with Thermal conductivity of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Electrical
Chemical properties
Property | Value | Related Standards |
---|---|---|
Aluminium | 10.5 - 11.5 % Show Material materials with Aluminium of 10.5 - 11.5 % | ASTM B505 |
Copper | 74.5 % Show Material materials with Copper of 74.5 % | ASTM B505 |
Iron | 4 - 5.5 % Show Material materials with Iron of 4 - 5.5 % | ASTM B505 |
Lead | 0.03 % Show Material materials with Lead of 0.03 % | ASTM B505 |
Manganese | 1.5 % Show Material materials with Manganese of 1.5 % | ASTM B505 |
Nickel | 4.2 - 6 % Show Material materials with Nickel of 4.2 - 6 % | ASTM B505 |
Silicon | 0.15 % Show Material materials with Silicon of 0.15 % | ASTM B505 |
Tin | 0.25 % Show Material materials with Tin of 0.25 % | ASTM B505 |
Zinc | 0.3 % Show Material materials with Zinc of 0.3 % | ASTM B505 |