ASTM B505 Grade C99500

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by ASTM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation A50

23.0 °C

12 %

Show Material materials with Elongation A50 of 12 %

Tensile strength

23.0 °C

483 MPa

Show Material materials with Tensile strength of 483 MPa

Yield strength Rp0.5

23.0 °C

276 MPa

Show Material materials with Yield strength Rp0.5 of 276 MPa

Chemical properties

PropertyValue

Aluminium

0.5 - 2 %

Show Material materials with Aluminium of 0.5 - 2 %

Iron

3 - 5 %

Show Material materials with Iron of 3 - 5 %

Lead

0.09 %

Show Material materials with Lead of 0.09 %

Manganese

0.5 %

Show Material materials with Manganese of 0.5 %

Nickel

3.5 - 5.5 %

Show Material materials with Nickel of 3.5 - 5.5 %

Silicon

0.5 - 2 %

Show Material materials with Silicon of 0.5 - 2 %

Zinc

0.5 - 2 %

Show Material materials with Zinc of 0.5 - 2 %