General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 8.47 g/cm³ Show Material materials with Density of 8.47 g/cm³ | Typical for Cast Copper Brass Yellow Brass |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 110 - 130 GPa Show Material materials with Elastic modulus of 110 - 130 GPa | Typical for Cast Copper Brass Yellow Brass |
Elongation A50 | 23.0 °C | 20 % Show Material materials with Elongation A50 of 20 % | |
Poisson's ratio | 23.0 °C | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Brass Yellow Brass |
Tensile strength | 23.0 °C | 207 MPa Show Material materials with Tensile strength of 207 MPa | |
Yield strength Rp0.5 | 23.0 °C | 97 MPa Show Material materials with Yield strength Rp0.5 of 97 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.5E-5 - 1.9E-5 1/K | Typical for Cast Copper Brass Yellow Brass |
Melting point | 905 - 932 °C Show Material materials with Melting point of 905 - 932 °C | Typical for Cast Copper Brass Yellow Brass | |
Specific heat capacity | 23.0 °C | 335 - 390 J/(kg·K) Show Material materials with Specific heat capacity of 335 - 390 J/(kg·K) | Typical for Cast Copper Brass Yellow Brass |
Thermal conductivity | 23.0 °C | 116 W/(m·K) Show Material materials with Thermal conductivity of 116 W/(m·K) | Typical for Cast Copper Brass Yellow Brass |
Chemical properties
Property | Value |
---|---|
Aluminium | 5E-3 % Show Material materials with Aluminium of 5E-3 % |
Antimony | 0.25 % Show Material materials with Antimony of 0.25 % |
Copper | 84 - 86 % Show Material materials with Copper of 84 - 86 % |
Iron | 0.3 % Show Material materials with Iron of 0.3 % |
Lead | 4 - 6 % Show Material materials with Lead of 4 - 6 % |
Nickel | 1 % Show Material materials with Nickel of 1 % |
Phosphorus | 0.05 % Show Material materials with Phosphorus of 0.05 % |
Silicon | 5E-3 % Show Material materials with Silicon of 5E-3 % |
Sulfur | 0.08 % Show Material materials with Sulfur of 0.08 % |
Tin | 4 - 6 % Show Material materials with Tin of 4 - 6 % |
Zinc | 4 - 6 % Show Material materials with Zinc of 4 - 6 % |