Mechanical
Chemical properties
Property | Value |
---|---|
Aluminium | 5E-3 % Show Material materials with Aluminium of 5E-3 % |
Antimony | 0.15 % Show Material materials with Antimony of 0.15 % |
Copper | 85 - 90 % Show Material materials with Copper of 85 - 90 % |
Iron | 0.25 % Show Material materials with Iron of 0.25 % |
Lead | 0.09 % Show Material materials with Lead of 0.09 % |
Manganese | 0.2 % Show Material materials with Manganese of 0.2 % |
Nickel | 4.5 - 6 % Show Material materials with Nickel of 4.5 - 6 % |
Phosphorus | 0.05 % Show Material materials with Phosphorus of 0.05 % |
Silicon | 5E-3 % Show Material materials with Silicon of 5E-3 % |
Sulfur | 0.05 % Show Material materials with Sulfur of 0.05 % |
Tin | 4.5 - 6 % Show Material materials with Tin of 4.5 - 6 % |
Zinc | 1 - 2.5 % Show Material materials with Zinc of 1 - 2.5 % |