Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 120 - 156 GPa Show Material materials with Elastic modulus of 120 - 156 GPa | Typical for Cast Copper Nickel Grade |
Elongation A50 | 23.0 °C | 3 % Show Material materials with Elongation A50 of 3 % | |
Poisson's ratio | 23.0 °C | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Nickel Grade |
Tensile strength | 23.0 °C | 862 MPa Show Material materials with Tensile strength of 862 MPa | |
Yield strength Rp0.2 | 23.0 °C | 689 MPa Show Material materials with Yield strength Rp0.2 of 689 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K | Typical for Cast Copper Nickel Grade |
Melting point | 1100 - 1240 °C Show Material materials with Melting point of 1100 - 1240 °C | Typical for Cast Copper Nickel Grade | |
Specific heat capacity | 23.0 °C | 377 J/(kg·K) Show Material materials with Specific heat capacity of 377 J/(kg·K) | Typical for Cast Copper Nickel Grade |
Thermal conductivity | 23.0 °C | 23 - 45 W/(m·K) Show Material materials with Thermal conductivity of 23 - 45 W/(m·K) | Typical for Cast Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.1 % Show Material materials with Aluminium of 0.1 % |
Antimony | 0.02 % Show Material materials with Antimony of 0.02 % |
Bismuth | 1E-3 % Show Material materials with Bismuth of 1E-3 % |
Iron | 0.5 % Show Material materials with Iron of 0.5 % |
Lead | 5E-3 % Show Material materials with Lead of 5E-3 % |
Manganese | 0.05 - 0.3 % Show Material materials with Manganese of 0.05 - 0.3 % |
Nickel | 9.5 - 10.5 % Show Material materials with Nickel of 9.5 - 10.5 % |
Phosphorus | 5E-3 % Show Material materials with Phosphorus of 5E-3 % |
Silicon | 0.05 % Show Material materials with Silicon of 0.05 % |
Sulfur | 2.5E-3 % Show Material materials with Sulfur of 2.5E-3 % |
Tin | 7.5 - 8.5 % Show Material materials with Tin of 7.5 - 8.5 % |
Zinc | 1 % Show Material materials with Zinc of 1 % |