Mechanical
Chemical properties
Property | Value |
---|---|
Aluminium | 0.1 % Show Material materials with Aluminium of 0.1 % |
Antimony | 0.02 % Show Material materials with Antimony of 0.02 % |
Bismuth | 1E-3 % Show Material materials with Bismuth of 1E-3 % |
Iron | 0.5 % Show Material materials with Iron of 0.5 % |
Lead | 5E-3 % Show Material materials with Lead of 5E-3 % |
Manganese | 0.05 - 0.3 % Show Material materials with Manganese of 0.05 - 0.3 % |
Nickel | 9.5 - 10.5 % Show Material materials with Nickel of 9.5 - 10.5 % |
Phosphorus | 5E-3 % Show Material materials with Phosphorus of 5E-3 % |
Silicon | 0.05 % Show Material materials with Silicon of 0.05 % |
Sulfur | 2.5E-3 % Show Material materials with Sulfur of 2.5E-3 % |
Tin | 7.5 - 8.5 % Show Material materials with Tin of 7.5 - 8.5 % |
Zinc | 1 % Show Material materials with Zinc of 1 % |