Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 100 - 125 GPa Show Material materials with Elastic modulus of 100 - 125 GPa | Typical for Wrought Copper Brass |
Hardness, Rockwell B | 23.0 °C | 51 - 70 [-] Show Material materials with Hardness, Rockwell B of 51 - 70 [-] | |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 50 - 67 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 50 - 67 [-] | |
Shear modulus | 23.0 °C | 40 GPa Show Material materials with Shear modulus of 40 GPa | Typical for Wrought Copper Brass |
Tensile strength | 23.0 °C | 340 - 415 MPa Show Material materials with Tensile strength of 340 - 415 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Melting point | 875 - 1075 °C Show Material materials with Melting point of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Specific heat capacity | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Specific heat capacity of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Thermal conductivity | 23.0 °C | 100 - 234 W/(m·K) Show Material materials with Thermal conductivity of 100 - 234 W/(m·K) | Typical for Wrought Copper Brass |
Chemical properties
Property | Value |
---|---|
Copper | 89 - 92 % Show Material materials with Copper of 89 - 92 % |
Iron | 0.05 % Show Material materials with Iron of 0.05 % |
Lead | 0.09 % Show Material materials with Lead of 0.09 % |
Tin | 0.3 - 0.7 % Show Material materials with Tin of 0.3 - 0.7 % |