Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 96 - 120 GPa Show Material materials with Elastic modulus of 96 - 120 GPa | Typical for Cast Copper Bronze |
Elongation A50 | 23.0 °C | 12 % Show Material materials with Elongation A50 of 12 % | |
Hardness, Brinell | 23.0 °C | 150 [-] Show Material materials with Hardness, Brinell of 150 [-] | |
Poisson's ratio | 23.0 °C | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Bronze |
Tensile strength | 23.0 °C | 515 MPa Show Material materials with Tensile strength of 515 MPa | |
Yield strength Rp0.5 | 23.0 °C | 205 MPa Show Material materials with Yield strength Rp0.5 of 205 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.9E-5 1/K | Typical for Cast Copper Bronze |
Melting point | 760 - 1060 °C Show Material materials with Melting point of 760 - 1060 °C | Typical for Cast Copper Bronze | |
Specific heat capacity | 23.0 °C | 376 - 440 J/(kg·K) Show Material materials with Specific heat capacity of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Thermal conductivity | 23.0 °C | 12 - 81 W/(m·K) Show Material materials with Thermal conductivity of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Chemical properties
Property | Value |
---|---|
Aluminium | 10 - 11.5 % Show Material materials with Aluminium of 10 - 11.5 % |
Copper | 83 % Show Material materials with Copper of 83 % |
Iron | 3 - 5 % Show Material materials with Iron of 3 - 5 % |
Manganese | 0.5 % Show Material materials with Manganese of 0.5 % |
Nickel | 1.5 - 2.5 % Show Material materials with Nickel of 1.5 - 2.5 % |