ASTM B763 Grade C97600 Separately Cast Test Bars

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by ASTM.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

8.4 - 8.9 g/cm³

Show Material materials with Density of 8.4 - 8.9 g/cm³

Typical for Cast Copper Nickel Silver Grade

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

110 - 130 GPa

Show Material materials with Elastic modulus of 110 - 130 GPa

Typical for Cast Copper Nickel Silver Grade

Elongation A50

23.0 °C

10 %

Show Material materials with Elongation A50 of 10 %

Poisson's ratio

23.0 °C

0.32 [-]

Show Material materials with Poisson's ratio of 0.32 [-]

Typical for Cast Copper Nickel Silver Grade

Tensile strength

23.0 °C

276 MPa

Show Material materials with Tensile strength of 276 MPa

Yield strength Rp0.5

23.0 °C

117 MPa

Show Material materials with Yield strength Rp0.5 of 117 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.5E-5 - 1.9E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.5E-5 - 1.9E-5 1/K

Typical for Cast Copper Nickel Silver Grade

Melting point

1010 - 1180 °C

Show Material materials with Melting point of 1010 - 1180 °C

Typical for Cast Copper Nickel Silver Grade

Specific heat capacity

23.0 °C

377 J/(kg·K)

Show Material materials with Specific heat capacity of 377 J/(kg·K)

Typical for Cast Copper Nickel Silver Grade

Thermal conductivity

23.0 °C

22 - 29 W/(m·K)

Show Material materials with Thermal conductivity of 22 - 29 W/(m·K)

Typical for Cast Copper Nickel Silver Grade

Chemical properties

PropertyValue

Aluminium

5E-3 %

Show Material materials with Aluminium of 5E-3 %

Antimony

0.25 %

Show Material materials with Antimony of 0.25 %

Copper

63 - 67 %

Show Material materials with Copper of 63 - 67 %

Iron

1.5 %

Show Material materials with Iron of 1.5 %

Lead

3 - 5 %

Show Material materials with Lead of 3 - 5 %

Manganese

1 %

Show Material materials with Manganese of 1 %

Nickel

19 - 21.5 %

Show Material materials with Nickel of 19 - 21.5 %

Phosphorus

0.05 %

Show Material materials with Phosphorus of 0.05 %

Silicon

0.15 %

Show Material materials with Silicon of 0.15 %

Sulfur

0.08 %

Show Material materials with Sulfur of 0.08 %

Tin

3.5 - 4.5 %

Show Material materials with Tin of 3.5 - 4.5 %

Zinc

3 - 9 %

Show Material materials with Zinc of 3 - 9 %

Do you have a technical question or need more information about this material?

Post it as a comment below and receive answers from engineers and other community members.