Mechanical
Chemical properties
Property | Value |
---|---|
Aluminium | 0.5 - 2 % Show Material materials with Aluminium of 0.5 - 2 % |
Iron | 3 - 5 % Show Material materials with Iron of 3 - 5 % |
Lead | 0.09 % Show Material materials with Lead of 0.09 % |
Manganese | 0.5 % Show Material materials with Manganese of 0.5 % |
Nickel | 3.5 - 5.5 % Show Material materials with Nickel of 3.5 - 5.5 % |
Silicon | 0.5 - 2 % Show Material materials with Silicon of 0.5 - 2 % |
Zinc | 0.5 - 2 % Show Material materials with Zinc of 0.5 - 2 % |