Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 110 - 130 GPa Show Material materials with Elastic modulus of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Hardness, Rockwell B | 23.0 °C | 90 - 92 [-] Show Material materials with Hardness, Rockwell B of 90 - 92 [-] | |
Tensile strength | 23.0 °C | 550 - 897 MPa Show Material materials with Tensile strength of 550 - 897 MPa | |
Yield strength | 23.0 °C | 414 - 690 MPa Show Material materials with Yield strength of 414 - 690 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Melting point | 855 - 1090 °C Show Material materials with Melting point of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Specific heat capacity | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Specific heat capacity of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Electrical
Property | Value |
---|---|
Specific Electrical conductivity | 45 % IACS Show Material materials with Specific Electrical conductivity of 45 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.2 % Show Material materials with Aluminium of 0.2 % |
Beryllium | 0.2 - 0.6 % Show Material materials with Beryllium of 0.2 - 0.6 % |
Cobalt | 0.3 % Show Material materials with Cobalt of 0.3 % |
Iron | 0.1 % Show Material materials with Iron of 0.1 % |
Nickel | 1.4 - 2.2 % Show Material materials with Nickel of 1.4 - 2.2 % |
Silicon | 0.2 % Show Material materials with Silicon of 0.2 % |