General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 8.9 g/cm³ Show Material materials with Density of 8.9 g/cm³ | Typical for Wrought Copper Pure / Low Alloyed Copper |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 95 - 98 GPa Show Material materials with Elastic modulus of 95 - 98 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Elongation | 23.0 °C | 2 % Show Material materials with Elongation of 2 % | |
Poisson's ratio | 23.0 °C | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Shear modulus | 23.0 °C | 48 GPa Show Material materials with Shear modulus of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Tensile strength | 23.0 °C | 325 - 395 MPa Show Material materials with Tensile strength of 325 - 395 MPa | |
Yield strength Rp0.2 | 23.0 °C | 295 MPa Show Material materials with Yield strength Rp0.2 of 295 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper Pure / Low Alloyed Copper |
Melting point | 965 - 1100 °C Show Material materials with Melting point of 965 - 1100 °C | Typical for Wrought Copper Pure / Low Alloyed Copper | |
Specific heat capacity | 23.0 °C | 377 - 420 J/(kg·K) Show Material materials with Specific heat capacity of 377 - 420 J/(kg·K) | Typical for Wrought Copper Pure / Low Alloyed Copper |
Chemical properties
Property | Value |
---|---|
Copper | 99.9 % Show Material materials with Copper of 99.9 % |
Phosphorus | 0 - 0.01 % Show Material materials with Phosphorus of 0 - 0.01 % |
Tellurium | 0 - 0.02 % Show Material materials with Tellurium of 0 - 0.02 % |
Tin | 0 - 0.02 % Show Material materials with Tin of 0 - 0.02 % |