Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 110 - 130 GPa Show Material materials with Elastic modulus of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Elongation | 23.0 °C | 22 % Show Material materials with Elongation of 22 % | |
Tensile strength | 23.0 °C | 345 - 415 MPa Show Material materials with Tensile strength of 345 - 415 MPa | |
Yield strength Rp0.2 | 23.0 °C | 145 MPa Show Material materials with Yield strength Rp0.2 of 145 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Melting point | 855 - 1090 °C Show Material materials with Melting point of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Specific heat capacity | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Specific heat capacity of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.02 % Show Material materials with Aluminium of 0.02 % |
Cobalt | 0.3 - 1.3 % Show Material materials with Cobalt of 0.3 - 1.3 % |
Copper | 96 % Show Material materials with Copper of 96 % |
Iron | 1 - 2 % Show Material materials with Iron of 1 - 2 % |
Lead | 0.02 % Show Material materials with Lead of 0.02 % |
Phosphorus | 0.01 - 0.35 % Show Material materials with Phosphorus of 0.01 - 0.35 % |
Tin | 0.1 - 1 % Show Material materials with Tin of 0.1 - 1 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |