ASTM B888 Grade C19700 H06

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

110 - 130 GPa

Show Material materials with Elastic modulus of 110 - 130 GPa

Typical for Wrought Copper High Copper Alloy

Elongation

23.0 °C

2 %

Show Material materials with Elongation of 2 %

Tensile strength

23.0 °C

460 - 505 MPa

Show Material materials with Tensile strength of 460 - 505 MPa

Yield strength Rp0.2

23.0 °C

440 MPa

Show Material materials with Yield strength Rp0.2 of 440 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.6E-5 - 1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.8E-5 1/K

Typical for Wrought Copper High Copper Alloy

Melting point

855 - 1090 °C

Show Material materials with Melting point of 855 - 1090 °C

Typical for Wrought Copper High Copper Alloy

Specific heat capacity

23.0 °C

360 - 420 J/(kg·K)

Show Material materials with Specific heat capacity of 360 - 420 J/(kg·K)

Typical for Wrought Copper High Copper Alloy

Chemical properties

PropertyValue

Cobalt

0.05 %

Show Material materials with Cobalt of 0.05 %

Iron

0.3 - 1.2 %

Show Material materials with Iron of 0.3 - 1.2 %

Lead

0.05 %

Show Material materials with Lead of 0.05 %

Magnesium

0.01 - 0.2 %

Show Material materials with Magnesium of 0.01 - 0.2 %

Manganese

0.05 %

Show Material materials with Manganese of 0.05 %

Nickel

0.05 %

Show Material materials with Nickel of 0.05 %

Phosphorus

0.1 - 0.4 %

Show Material materials with Phosphorus of 0.1 - 0.4 %

Tin

0.2 %

Show Material materials with Tin of 0.2 %

Zinc

0.2 %

Show Material materials with Zinc of 0.2 %