Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 100 - 125 GPa Show Material materials with Elastic modulus of 100 - 125 GPa | Typical for Wrought Copper Brass |
Elongation | 23.0 °C | 15 % Show Material materials with Elongation of 15 % | |
Shear modulus | 23.0 °C | 40 GPa Show Material materials with Shear modulus of 40 GPa | Typical for Wrought Copper Brass |
Tensile strength | 23.0 °C | 305 - 370 MPa Show Material materials with Tensile strength of 305 - 370 MPa | |
Yield strength Rp0.2 | 23.0 °C | 160 MPa Show Material materials with Yield strength Rp0.2 of 160 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Melting point | 875 - 1075 °C Show Material materials with Melting point of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Specific heat capacity | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Specific heat capacity of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Thermal conductivity | 23.0 °C | 100 - 234 W/(m·K) Show Material materials with Thermal conductivity of 100 - 234 W/(m·K) | Typical for Wrought Copper Brass |