Property | Value |
---|---|
Aluminium | 9 - 12 % Show Material materials with Aluminium of 9 - 12 % |
Copper | 80 - 87 % Show Material materials with Copper of 80 - 87 % |
Iron | 3 - 5 % Show Material materials with Iron of 3 - 5 % |
Manganese | 0.5 - 2 % Show Material materials with Manganese of 0.5 - 2 % |
Nickel | 0.5 - 2 % Show Material materials with Nickel of 0.5 - 2 % |