JIS Z3231 Grade DCuSiA H58

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by Japanese Industrial Standards.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

22 %

Show Material materials with Elongation of 22 %

Tensile strength

23.0 °C

245 MPa

Show Material materials with Tensile strength of 245 MPa

Technological properties

Property
Processing history

drawn