General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 8.47 g/cm³ Show Material materials with Density of 8.47 g/cm³ | Typical for Cast Copper Brass Yellow Brass |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 110 - 130 GPa Show Material materials with Elastic modulus of 110 - 130 GPa | Typical for Cast Copper Brass Yellow Brass |
Elongation | 23.0 °C | 25 % Show Material materials with Elongation of 25 % | |
Poisson's ratio | 23.0 °C | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Cast Copper Brass Yellow Brass |
Tensile strength | 23.0 °C | 147 MPa Show Material materials with Tensile strength of 147 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.5E-5 - 1.9E-5 1/K | Typical for Cast Copper Brass Yellow Brass |
Melting point | 905 - 932 °C Show Material materials with Melting point of 905 - 932 °C | Typical for Cast Copper Brass Yellow Brass | |
Specific heat capacity | 23.0 °C | 335 - 390 J/(kg·K) Show Material materials with Specific heat capacity of 335 - 390 J/(kg·K) | Typical for Cast Copper Brass Yellow Brass |
Thermal conductivity | 23.0 °C | 116 W/(m·K) Show Material materials with Thermal conductivity of 116 W/(m·K) | Typical for Cast Copper Brass Yellow Brass |
Technological properties
Property | ||
---|---|---|
Processing history | as-cast |