Elongation A50 A50
0 - 22 % at 20 °C
Tensile strength Rm
0 - 330 MPa at 20 °C
Yield strength Rp0.5 Rp0.5
0 - 125 MPa at 20 °C
Element
Weight %
Comment
62 - 65 %
0.5 - 1 %
0 - 0.1 %
0 - 0.2 %
This material data has been provided by ASTM.