ASTM B21 Grade C46400 H02

.XLSX
.PDF
Save

Description

Related Standards

Properties

Mechanical

Elongation A50 A50

22 - 30 % at 20 °C

Hardness, Rockwell B HRB

55 - 80 [-] at 20 °C

Tensile strength Rm

370 - 415 MPa at 20 °C

Yield strength Rp0.5 Rp0.5

150 - 185 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

59 - 62 %

Sn

0.5 - 1 %

Pb

0.2 %

Fe

0.1 %

This material data has been provided by ASTM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.