General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 8.9 g/cm³ Show Material materials with Density of 8.9 g/cm³ | Typical for Wrought Copper Pure / Low Alloyed Copper |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 95 - 98 GPa Show Material materials with Elastic modulus of 95 - 98 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Hardness, Rockwell F | 23.0 °C | 50 [-] Show Material materials with Hardness, Rockwell F of 50 [-] | |
Hardness, Rockwell Superficial 15-T | 23.0 °C | 60 [-] Show Material materials with Hardness, Rockwell Superficial 15-T of 60 [-] | |
Poisson's ratio | 23.0 °C | 0.34 [-] Show Material materials with Poisson's ratio of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Shear modulus | 23.0 °C | 48 GPa Show Material materials with Shear modulus of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Tensile strength | 23.0 °C | 205 MPa Show Material materials with Tensile strength of 205 MPa | |
Yield strength Rp0.5 | 23.0 °C | 62 MPa Show Material materials with Yield strength Rp0.5 of 62 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper Pure / Low Alloyed Copper |
Melting point | 965 - 1100 °C Show Material materials with Melting point of 965 - 1100 °C | Typical for Wrought Copper Pure / Low Alloyed Copper | |
Specific heat capacity | 23.0 °C | 377 - 420 J/(kg·K) Show Material materials with Specific heat capacity of 377 - 420 J/(kg·K) | Typical for Wrought Copper Pure / Low Alloyed Copper |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 23.0 °C | 1.72E-8 Ω·m Show Material materials with Electrical resistivity of 1.72E-8 Ω·m |
Specific Electrical conductivity | 100 % IACS Show Material materials with Specific Electrical conductivity of 100 % IACS |
Chemical properties
Property | Value |
---|---|
Copper | 99.95 % Show Material materials with Copper of 99.95 % |